The latest from Lubinpla
More stories
-
Cooling tower acid overfeed crashed the pH: what to do now
After a cooling tower acid overfeed, stop the acid feed, raise blowdown, check metals and discharge limits, fix the controller and confirm recovery.
-
Bleach to chlorine dioxide in cooling towers: switching risks
Chlorine dioxide beats bleach in alkaline or ammonia-laden cooling water, but generator choice, chloride, copper and acid supply can trip a switch.
-
ASTM D1748 Humidity Cabinet Results: What Pass and Fail Predict
ASTM D1748-24 rates rust dots on coated steel panels after set humidity cabinet hours. A pass ranks similar preservatives; it cannot predict storage life.
-
Tankside Biocides and CNC Machine Coolant Emulsion Stability
A tankside biocide splits a CNC coolant emulsion only when overdosed, mismatched to the coolant or poorly mixed. Check dose, pH and a jar test first.
-
Coolant Concentrate Separated in the Drum: When It Is Usable
Separated coolant concentrate is usable only if stirring at room temperature restores one phase and a test dilution stays stable. When to reject the drum.
-
Coolant dip slide test results at 10^6: what to do next
A coolant dip slide at 10^6 CFU/mL means poor bacterial control. Confirm the reading, check the fluid, decide to treat or drain, then retest to close it.
-
Metalworking coolant gone bad: what to ask on the first call
Ask six things on a coolant problem call: the symptom, machine and material, recent changes, concentration and pH, top-up practice, and samples to bring.
-
Coolant Problems: Distributor Fix vs Supplier Technical Support
Keep a coolant problem with the distributor when concentration, pH or contamination checks explain it; escalate when the product itself is suspect.
-
Magnesium machining coolant: choosing for hydrogen and pH drift
For magnesium machining, use a pH-buffered magnesium-rated water-miscible coolant for output, or neat oil where fines and hydrogen must be avoided.
-
Why Coolant Concentration Keeps Dropping in the Sump
Falling coolant concentration usually comes from a wrong refractometer factor, drag-out on parts and chips, or lean makeup. How to tell them apart on site.
Talk to us about your sales team.
Custom plans, custom terms, security reviews and onboarding across teams or branches. Tell us a little about your organization and we will reply with a starting plan.
Contact Sales- 01Start from site data and your documents
Bring in the TDSs, test reports and site records your team already has. Where a case has too little to go on, the agent searches the web for public sources such as manufacturer data and standards.
- 02State the case
Describe the customer's situation in plain words. The agent reads the site's conditions and history, proposes the task that fits, and starts when you say go.
- 03Review the reasoning, step by step
Each step shows what was considered, what the evidence supports and what was ruled out, with the source behind each point. You can carry on, ask for changes or stop.
- 04One document for this customer
The case ends in a document built for that customer: the conclusion, the reasoning, the conditions it depends on and what to do next. Share it through Field Care when you choose.